| Test | Standard | Results | Implication |
| Abrasion | ASTM D4060 | C5-10 wheel / 1 kg load
1000 cycles <100 mg | High levels of abrasion resistance |
| Adhesion | ISO 4624 | >5 MPa
(7 days cured) | Excellent corrosion protection |
| Condensation | ASTM D4585 | No blisters, rust or crack after 6,000 hrs exposure. Excellent adhesion | Excellent corrosion protection |
| Elongation | ASTM D2370 | >2% | Tolerates deformation |
Hardness,
Barcol | ASTM D2583 | 40-50 | High levels of wear resistance |
| Impact resistance | ASTM D2794 | >18 J | Tolerates deformation |
| Salt spray | ASTM B117 | No blisters, rust or crack after 10,000 hrs exposure. Excellent adhesion | Excellent corrosion protection |
| Tensile strength | ASTM D23270 | >10 MPa | Tolerates deformation |